Guide ·
FEP-Encapsulated O-Rings: A Practical Guide to Silicone vs. Viton Cores
An FEP-encapsulated O-ring is a compromise that works. It has a thin seamless jacket of FEP (fluorinated ethylene propylene) around an elastomer core, usually silicone or FKM, which many people call Viton after the Chemours trade name. The jacket handles the chemistry. The core provides the elasticity that a fluoropolymer lacks. If you have been asked to seal a line that runs acids on Monday, solvents on Wednesday and steam on Friday, these rings are worth understanding properly.
This guide covers how encapsulated rings behave, how to choose between silicone and FKM cores, the groove and installation details that decide whether they last, and when a solid PTFE ring is still the better answer.
Why encapsulate at all?
PTFE and FEP resist almost every chemical. The main exceptions are molten alkali metals, elemental fluorine and a few exotic fluorinating agents. Both fluoropolymers have poor elastic recovery, though. Squeeze a solid PTFE ring and much of the deformation stays. Over time the material cold-flows away from the load and sealing force drops. That is fine in some static joints and a real problem in others.
Elastomers have the opposite profile. They recover well, but each compound is attacked by something: silicone by many solvents and steam over time, FKM by ketones, amines and hot water, EPDM by oils. An encapsulated ring puts the elastomer inside a chemically inert jacket, so the energising core never touches the media as long as the jacket is intact.

The jacket: FEP or PFA?
Most encapsulated rings use FEP. It can be melt-processed into a seamless tube, it is fully transparent (useful for inspection) and it is accepted in food and pharmaceutical service. In the US, perfluorocarbon resins in food contact are covered by 21 CFR 177.1550. FEP’s continuous service limit is around +205 °C.
PFA jackets are available for hotter service, up to about +260 °C. They cost more, are less flexible and are harder to stretch during installation. Unless the temperature requires PFA, FEP is the default.
Silicone core vs. FKM core
This is the decision that matters most. Both cores sit behind the same jacket, but they behave differently once the joint has been in service for a few months.
FEP over silicone
- Typical range: about −60 °C to +205 °C
- Strengths: good low-temperature flexibility and a soft feel that seats well in hygienic clamp joints. Usually the cheaper option.
- Weaknesses: lower tear strength, and more compression set at sustained high temperature than FKM.
- Best for: food, dairy, beverage and pharmaceutical equipment, cryogenic or cold-room duty, and static joints that are opened often.
Silicone is usually the right default for hygienic process plants. The temperature span covers CIP cycles, the soft core forgives slightly imperfect clamp ferrules, and if a jacket is ever breached, silicone is generally acceptable in those industries anyway.
FEP over FKM (Viton)
- Typical range: about −20 °C to +200 °C
- Strengths: better compression-set resistance at heat, higher mechanical strength, and good resistance to fuels, oils and many solvents.
- Weaknesses: stiffer at low temperature, harder to install in small cross-sections, and FKM itself dislikes ketones, esters and hot water.
- Best for: chemical process pumps, mechanical seal secondary seals, hydrocarbon service and continuously hot static joints.
FKM matters most when the jacket fails. If an aggressive solvent gets through a jacket nicked at installation, a silicone core can swell and break down quickly. An FKM core tolerates hydrocarbons better, so you get slow weeping, which you can see and plan around, instead of a sudden loss of sealing force.
Quick comparison
| Property | FEP / silicone | FEP / FKM |
|---|---|---|
| Low temperature | about −60 °C | about −20 °C |
| High temperature | about +205 °C | about +200 °C |
| Compression set at heat | Moderate | Good |
| Behaviour if jacket breached by solvent | Poor | Better |
| Typical sectors | Food, pharma, cryogenic | Chemical, petrochemical, pumps |
These are typical published ranges. Always check the specific supplier’s datasheet, because jacket thickness and core compound affect the limits.
Solid core, hollow core and other variants
Most rings have a solid elastomer core. Hollow silicone cores reduce installation force and suit fragile or plastic housings, but they give lower sealing force. Some manufacturers also offer stainless steel spring cores for cryogenic or very high-temperature duty, where no elastomer would survive. If your housing is glass-lined, PEEK or thin-walled, ask about hollow cores.
Sizing: metric, AS568 and the large diameters
Encapsulated rings come in the same dash sizes as ordinary O-rings. In North America and in a lot of imported equipment, that means the AS568 inch series. European housings more often use metric sizes to ISO 3601 or simply “inside diameter × cross-section” in millimetres. A ring described as Ø78.97 × 3.53 is an AS568 size expressed in millimetres. A ring described as Ø24.0 × 2.5 is a true metric size. Confusing the two is a common reason a “correct” replacement will not seat.
Because the jacket is made from extruded tube and joined into a ring, large diameters are not a problem. Rings over a metre in diameter are routine for manway covers, reactor lids and large filter housings. The limits are at the small end. Below about 2 mm cross-section, or with very small inside diameters, the jacket becomes hard to form and the ring stiff to fit. If the design allows it, go up one cross-section size.
Groove design: where most failures start
Encapsulated rings are less elastic than plain elastomer rings. The jacket stretches very little before it creases or splits. That has three practical consequences:
- Prefer open or split grooves. In closed glands, installation stretch should stay under about 2–3 %. With a plain elastomer you could stretch much further.
- Use standard O-ring squeeze, not PTFE squeeze. About 10–20 % for static seals is typical. Too little and the jacket will not conform. Too much and the jacket creases permanently.
- Break every edge. Burrs, thread crests and sharp groove corners are the main causes of nicked jackets. Radius groove corners and chamfer lead-in edges at 15–20°.
Encapsulated rings suit static or slow-moving applications. They handle slow reciprocating or low-speed rotary duty, but they are not a substitute for a dedicated dynamic seal in fast-cycling cylinders.

Installation without damage
Most short service lives come from installation damage. A good routine:
- Warm the ring in hot water at around 80 °C for a few minutes before fitting. FEP becomes noticeably more pliable and you avoid creasing.
- Use a cone or sleeve over threads and sharp shoulders. Never roll the ring over a thread.
- Do not twist. A twisted jacket leaves a spiral crease that turns into a leak path.
- Let it recover. After stretching onto a piston, allow a few minutes (or a short warm-up) for the ring to shrink back before closing the housing.
- Lubricate if allowed by the process. A compatible lubricant reduces friction during assembly but is not needed for sealing.
Inspect the ring through the transparent jacket before fitting. Bubbles, a visible core gap or a jacket seam on a “seamless” ring are reasons to reject it.
When solid PTFE is still the better choice
Encapsulated rings are not always the answer. Solid PTFE O-rings handle −200 °C to +260 °C and are fully inert throughout. That suits static joints at the extremes of temperature or chemistry, or applications where any elastomer is prohibited. You will need tighter surface finishes, more bolt load and probably a re-torque after the first heat cycle. Filled PTFE grades (glass, carbon, bronze) reduce cold flow at the cost of some chemical resistance.
For flat flange joints, a gasket of expanded PTFE is often more practical than any O-ring. It conforms to uneven surfaces and creeps far less than virgin PTFE sheet.
Troubleshooting: reading a failed ring
A failed encapsulated ring usually tells you why it failed. Before you fit a replacement, look at the old one:
- A clean cut or split in the jacket usually means installation damage, such as a thread, a burr or a sharp groove edge. Fix the hardware, not the ring.
- A permanent flat on both faces with no other damage suggests too much squeeze or long exposure at the top of the temperature range. Check the gland depth, or move from silicone to FKM.
- A wrinkled or creased jacket points to too much stretch during installation, or a ring that is too large for the groove and has bunched up.
- A swollen, soft or discoloured core visible through the jacket means the media has reached the core. Look for a pinhole, then reconsider the core material for that media.
- A leak but a perfect-looking ring usually means surface finish or flange flatness. Fluoropolymer jackets need smoother sealing faces than soft elastomers. Around Ra 0.4–0.8 µm is a common target for static faces.
Keep failed rings in a labelled bag along with the operating history. A small collection of failures teaches a maintenance team more than any chart.
Frequently asked questions
Are FEP-encapsulated rings the same as “Teflon O-rings”? Not quite. “Teflon” is a brand name used loosely for PTFE, FEP and PFA. A solid PTFE O-ring and an FEP-encapsulated O-ring behave very differently, so always specify the construction, not only the brand.
Can I reuse an encapsulated ring? In non-critical static joints, sometimes, if it shows no creasing or flattening. In hygienic or hazardous service, treat them as single-use. The jacket takes a set that will not seal as well a second time.
Do they work in steam? FEP itself handles steam well within its temperature limit. Silicone cores do not like prolonged steam if the jacket is breached, and FKM is poor in hot water and steam. For steam-heavy duty, keep jackets undamaged and replace on a schedule.
A note on PFAS regulation
FEP, PFA and PTFE are all fluoropolymers, so they fall within the broad PFAS definition used in the EU universal PFAS restriction proposal that five European countries submitted to ECHA in 2023. Industrial seals are part of that discussion, and suppliers are already asking customers about critical-use cases. If you are standardising on encapsulated rings for a new plant, keep an eye on how the process develops and record why fluoropolymers are needed in each position. That record will help if derogations are needed later.
What they cost, and when that is justified
An encapsulated ring typically costs several times as much as a standard FKM or EPDM ring of the same size, and large diameters cost considerably more. That price makes sense when one ring replaces several elastomer grades on a multi-product line, or when a single failure means a scrapped batch, a confined-space entry or a regulatory report. It does not make sense in a clean water line or a lube-oil circuit, where a standard elastomer will last just as long.
Calculate the cost per year of service, not the price per ring. Include the downtime for each change-out, and the encapsulated ring often comes out cheaper in aggressive duty. Where the chemistry is mild and the joint is easy to reach, a well-chosen plain elastomer is still the sensible choice.
Ordering checklist
Before you send the purchase order, confirm:
- Inside diameter and cross-section (metric or AS568 inch series)
- Jacket material: FEP or PFA
- Core: solid silicone, solid FKM, hollow silicone or spring
- Required compliance documents (FDA, EU 1935/2004, USP Class VI, ATEX if relevant)
- Media at its worst concentration and temperature, including cleaning cycles
- Static, reciprocating or rotary duty
With those six answers you can order the right ring the first time. If the joint is part of a hose or transfer line, read the PTFE hose selection checklist as well. If you need to bond a PTFE component near the seal, see our guide to etching PTFE for bonding.